Skip to main content

Table 6 Changes in absolute amounts of detergent fiber (g) over an eight wk period of 0.5 and 2 cm wheat straw incubated with three different amounts of L. edodes inoculum

From: The effect of particle size and amount of inoculum on fungal treatment of wheat straw and wood chips

Particle size

0.5 cm

2 cm

Inoculum, %

0.5

1.5

3

0.5

1.5

3

 

Wk

      

ADL

0

17.7a

17.7ab

17.7a

17.7b

17.7a

17.7a

 

2

18.4a

19.5a

19.2a

20.6a

18.8a

18.0a

 

4

17.5a

18.3ab

16.0ab

16.8b

15.2b

15.2b

 

6

15.7ab

15.2b

18.3a

12.7c

12.0c

12.2c

 

8

14.6b

14.7b

13.2b

10.4d

10.1d

9.7d

SEM

0.60

0.85

0.77

0.33

0.32

0.43

P-value

0.0062

0.0113

0.0019

<.0001

<.0001

<.0001

HC

0

56.0a

56.0a

56.0a

56.0a

56.0a

56.0a

 

2

55.6a

54.0a

51.6ab

55.2a

52.8a

51.1b

 

4

47.9b

50.1ab

45.6c

49.8a

46.3b

44.7c

 

6

43.1c

43.2bc

47.3bc

39.3b

38.2c

36.1d

 

8

44.8bc

41.7c

41.8c

36.8b

34.8c

36.4d

SEM

0.96

1.49

1.29

1.59

0.92

0.64

P-value

<.0001

0.0001

0.0001

<.0001

<.0001

<.0001

Cell

0

92.5

92.5ab

92.5

92.5

92.5

92.5

 

2

92.5

91.4b

90.6

94.9

91.7

91.1

 

4

92.6

96.6a

94.0

90.9

95.5

93.5

 

6

94.7

92.8ab

91.6

93.2

92.9

95.1

 

8

91.2

89.5b

90.3

93.6

93.9

91.7

SEM

1.38

1.03

1.08

1.59

0.83

1.06

P-value

0.5141

0.0076

0.1953

0.5183

0.0667

0.1257

  1. Values with different superscripts within column are significantly (P < 0.05) different. ADL acid detergent lignin, HC hemicellulose, Cell cellulose, SEM standard error of the mean